OL 20

Liquid Photopolymer Application

Corrugated Printing Plate M20 is ideally suitable for corrugate cardboard
printing, especially the fluted corrugated surface.
Mypol 20 is designed with a lower hardness level of
18 ShoreA, ideal for corrugate cardboard with Technical Specification
fluted corrugated surface. This product delivers Packaging: product will be delivered in plastic UV
tack free plate surface and high quality solid protected IBC tanks of 1000 Kg, 200kg steel drums
coverage on printing. The Mypol 20 is formulated or 18 kg pails or jerry cans.
with the aliphatic product to prevent the yellowing Product warranty : The product is recommended to
of plates. be used within 12 months from its production date.
It must be stored in adequate temperature and
The Mypol 20 is available in transparent colour protected from light and heat. Warranty is valid for
(colourless). 12 months + transport time.

Key Features REPRODUCIBILITY :
Points net (half tone dot area) 3-95% at 40 lines/cm
Tack free printing plate for high quality solid (100 l/inch)
coverage Thin (fine) lines : 0,18 mm (0,007 inch) in width
Good resilience and excellent ink transfer
Wide imaging latitudeensures the best result in PLATE PROCESSING
fine detail printing M20 is available with hardness 18 Shore A.
Excellent durability, UV and thermal stability Viscosity 30,000 – 40,000 mPa x sec at 25 deg
Non-yellowing formula celcius
Appearance Colourless

*For a better performance we recommend printing
plates to be stored at temperature between 10 and
30 degrees Celsius, with relative humidity at 60%.
Plates should be protected from sun and UV light.

INDICATIVE TREATMENTS TIME RECOMENDATION

(Plate times changes according to thickness and

different type of equipment used for production)

INDICATIVE TIME 2,84 mm 3.94 mm

Pre-exposure t3h0icskenceosnsds t4h0icskenceosnsds

Main exposure 190 seconds 240 seconds

Washing 10 minutes 10 minutes

wet exposure 10-20 minutes 10-20 minutes

*Wet exposure beyond the recommended timing
may affect the finished goods performance and
durability.